查詢結果分析
相關文獻
- The Codeposition of Molybdenum Disulfide with Nickel: Process and Electrocatalytic Characteristics
- Functional Behavior of Particle-Volume-Graded Electrodeposited Composite Coatings
- Recent Advances in the Synthesis and Properties of Amorphous and Crystalline Carbon Nitride
- Continuous Fiber Reinforced Ceramic Composites
- 鍍層後處理對鍍鋅鋼片點銲疲勞性影響
- 物理蒸鍍單層及複層氮化鈦中碳鋼之拉伸及疲勞性質
- 裝飾性金屬件--電鍍製程設計及鍍層後處理
- Voltammetric Investigation of Nickel-Platinum Codeposits for Methanol Oxidation in KOH Solutions
- 金屬表面檢驗﹣﹣鍍層厚度測定
- The Effect of Coating Film on the Thermal Stress of Metal Matrix Composite
頁籤選單縮合
| 題 名 | The Codeposition of Molybdenum Disulfide with Nickel: Process and Electrocatalytic Characteristics=鎳-二硫化鉬複合電鍍的程序及鍍層特性研究 |
|---|---|
| 作 者 | 張瑩崟; 林俊一; 張裕祺; | 書刊名 | Journal of the Chinese Institute of Chemical Engineers |
| 卷 期 | 28:4 1997.07[民86.07] |
| 頁 次 | 頁245-252 |
| 分類號 | 472.16 |
| 關鍵詞 | 鎳-二硫化鉬; 複合電鍍; 鍍層; Composite electrodeposition; Ni-MoS[feaf]; HER catalyst; |
| 語 文 | 英文(English) |
| 中文摘要 | 本研究應用實驗計畫法探究鎳-二硫化鉬複合電鍍的程序特性。就所選定的五項因子言,實驗數據經統計分析顯示鍍液溫度及pH為具顯著性的因子,而電極轉速則為次要因子。實驗結果示明鍍層中二硫化鉬含量隨pH上升而增大,但隨鍍液溫度上升而下降。本研究所製得的複合鍍層經在鹼性溶液中測試,證明其析氫催化能力優於純銅及純鎳鍍層,且當複合鍍層中二硫化鉬重量含量約34%時,催化活性最優。 |
| 英文摘要 | Composites containing molybdenum disulfide of various contents in a nickel matrix were prepared using composite electrodeposition technique in this study. The nickel- molybdenum disulfide system, as a hydrogen electrode in alkaline solutions, exhibited a more significant increase in electrocatalytic property than pure copper and electrodeposited nickel. Moreover, the electrocatalytic performance displayed an optimum efficiency at 34% by weight of the MoS₂ in deposit. We also examined the process characteristics of codepositing MoS₂ particles with nickel using statistical experimental design in order to obtain a better understanding of the process. The critical factors in codepositing nickel and molybdenum disulfide particles were investigated. According to those results, the pH value and bath temperature are of primary importance. Rotation rate of electrode is a secondary significant factor. The extent of code-position increases with the pH value of the bath. The extent of incorporating the MoS₂ phase, however, decreases with the solution's temperature. |