題名 | 壓鑄鎂合金之耐潛變性質與顯微結構=Creep Resistant Properties and Microstructure of Die Cast Magnesium Alloys |
---|---|
作者姓名(中文) | 黃維毅; 邱傳聖; 許光良; 洪衛朋; | 書刊名 | 鑄造工程學刊 |
卷期 | 33:4=135 2007.12[民96.12] |
頁次 | 頁25-30 |
關鍵詞 | 高溫鎂合金; 抗潛變; 鬆弛角度; 高溫性質; High-temperature magnesium alloys; Creep-resistance; Relax angle; Elevated temperatures; |
語文 | 中文(Chinese) |
中文摘要 | 本研究使用類似潛變的螺栓緊固力鬆弛法,測試AZ91D、AZC912、AM60B、AMCa602、ZA124等五種材料的耐潛變強度並探討其顯微結構,因為在許多鎂合金的使用場合鬆弛情形的現象會比潛變來的多,例如螺栓或是零件接合處。本實驗以五種材料在四個不同溫度參數:常溫、150℃、175℃與200℃,受到固定的扭力荷重作用下,比較鬆弛的扭轉角度,並探討其高溫耐潛變特性、顯微結構及機械性質之關係。 |
英文摘要 | This study analyzed about creep resistant which uses Bolt-Load-Loss method to test the materials of AZ91D, AZC912, AM60B, AMCa602, ZA124.These five kinds of materials were supported certain torsion load capacity at four temperature parameters: 25℃, 150℃, 175℃and 200℃, respectively. The reverse angle of relaxes under different temperature and torsion was compared with their interrelation with micro-structural features and mechanical properties. |